Difficulties in cutting titanium alloy structural parts
1.1 High cutting temperature
Because the thermal conductivity of titanium alloy materials is small (about 1/3 to 1/6 of steel), high cutting temperatures are easily generated when processing titanium alloys. Under the same conditions, the cutting heat generated by processing titanium alloy is more than twice as high as that of the same steel, and the heat generated by processing is difficult to be released through the workpiece. The specific heat coefficient of titanium alloy is small, and the local temperature rises quickly during processing, so it is easy to cause the instantaneous temperature of the tool to be too high, causing the tool tip to wear rapidly, and even overburning occurs.

1.2 High cutting resistance
The cutting force when cutting titanium alloy is basically the same as that when cutting steel, so the energy consumed during the cutting process is the same or slightly lower than that of steel. But when cutting titanium alloys, the stress near the main cutting edge is very high. This may be due to the fact that the chip contact area on the rake surface is usually very small when cutting titanium alloy (about 1/3 of cutting steel under the same conditions), and the large cutting stress causes the workpiece to yield during the machining process. phenomenon, the size of the processed workpiece is inconsistent.

1.3 Tremor of weakly rigid structures
Chatter is an important problem that needs to be overcome when processing weakly rigid structural parts of titanium alloys. Especially during finishing, the low elastic modulus of titanium alloys is the primary cause of vibration during the cutting process. When subjected to cutting forces, titanium alloys deform twice as much as carbon steel. The friction between the rebound of the flank surface and the machined surface produces vibration, and at the same time, a high cutting temperature is generated. Part of the cause of chatter is the high dynamic cutting force when cutting titanium alloys, which can reach more than 30% of the static force. This is due to the plastic shearing process during titanium alloy chip formation. Due to the influence of cutting chatter, the surface quality of the milled workpiece is difficult to meet the accuracy requirements.