Preparation Method Of Silicon Barium

Silicon-barium (Si-Ba) alloy is commonly used as a deoxidizer and desulfurizer in steelmaking and as an inoculant in casting. The preparation of Si-Ba alloy generally involves carbothermal reduction or aluminothermic reduction in an electric arc furnace or submerged arc furnace. The main methods are as follows:

1. Carbothermal Reduction Method

This is the most widely used method for producing silicon-barium alloy. The process involves reducing barium-containing minerals (such as barite, BaSO₄) and silica (SiO₂) with carbon at high temperatures.

Reaction equation:

BaSO4+4C→BaS+4CO↑BaSO_4 + 4C \rightarrow BaS + 4CO\uparrowBaSO4​+4C→BaS+4CO↑ BaS+SiO2+2C→BaSi+2CO↑BaS + SiO_2 + 2C \rightarrow BaSi + 2CO\uparrowBaS+SiO2​+2C→BaSi+2CO↑

Process steps:

Raw material preparation: Mix barite (BaSO₄), quartz (SiO₂), and coke (C) in specific proportions.

Smelting: The mixture is fed into an electric arc furnace at 1400–1600°C, where reduction reactions occur.

Alloy separation: The molten Si-Ba alloy is separated from slag and impurities.

Casting and cooling: The alloy is cast into ingots and cooled before crushing into required particle sizes.


2. Aluminothermic Reduction Method

This method uses aluminum (Al) as a reducing agent instead of carbon. It is typically used for high-purity Si-Ba production.

Reaction equation:

3BaO+2Al→3Ba+Al2O33BaO + 2Al \rightarrow 3Ba + Al_2O_33BaO+2Al→3Ba+Al2​O3​ Ba+Si→BaSiBa + Si \rightarrow BaSiBa+Si→BaSi

Process steps:

Mixing: Barite (BaO), silicon dioxide (SiO₂), and aluminum powder are blended in precise ratios.

Ignition: The mixture is ignited at high temperatures (~2000°C) to trigger a highly exothermic reaction.

Separation: The molten Ba-Si alloy separates from aluminum oxide (Al₂O₃) slag.

Cooling & Processing: The solidified alloy is crushed into granules or powders as needed.


3. Electrolytic Reduction Method (Less Common)

Involves the electrolysis of barium salts and silica in molten electrolytes.

High-purity Si-Ba alloys can be obtained, but this method is costly and less commonly used in industrial applications.