How To Take Ferrosilicon Sample Correctly?

Ferrosilicon standards specify the fluctuation range of the silicon content of ferrosilicon. Whether the ferrosilicon sampling method is correct or not, that is, how representative the sampling is, is directly related to the determination of product quality.

Ferro silicon 75 manufacturers

Practice shows that ferrosilicon should be sampled during the pouring process so that its silicon content is representative and its degree of segregation is small. It is not possible to take samples from the taphole or from the molten iron ladle.

Ferro silicon 75 suppliers

Larger-capacity submerged arc furnaces smelt 75% ferrosilicon, generally requiring two pours. For the first pouring, take a sample from each of the two middle molds. For the second pouring, take a sample from each of the two middle molds. Mix these samples together to make the total sample for this furnace. The composition of the samples taken in this way is representative, because the first sample is exactly the molten iron in the middle of the upper half of the molten iron ladle, and the second sample is exactly the molten iron in the middle of the lower half of the molten iron ladle.

Ferro silicon 75 factory

To smelt 45 ferrosilicon, one casting is required and a liquid sample is taken from the middle ingot mold.

 

Carbon sample spoons and molds should be used when sampling to prevent the liquid ferrosilicon from melting the sample spoon and affecting the accuracy of analysis.

 

If the liquid cannot be read, a cylinder sample can be taken at the midpoint of three or four bisectors of the diagonal line of the ferrosilicon ingot. The weight of each point should be roughly equal, and then mixed together to serve as the total sample of the iron in this furnace. Sample.