Raw material synthesis and production
Tertiary grade bauxite clinker and pyrophyllite are used as refractory aggregates, light high alumina or light mullite as aggregate, fine sand as bauxite clinker, αAl2O3 and SiO2 as ultrafine powder, and CA-50 steel as concluding agent and polyphosphate as abatement soup agent. The top or first grade alumina clinker is used as refractory aggregate and powder, the latter with mullite powder as part of the raw material, adding composite super micro powder, and CA-70 steel as concluding agent and soup reducing agent.

Alumina 88%>88% bauxite clinker as refractory aggregate, alumina-based spinel (Al2O362% and MgO_MgO_MgO), alumina containing more than 95% of magnesia sand and α-Al2O3 ultrafine powder as refractory powders, and alumina containing 93% of - Sodium sulphate as a concluding agent and fat reducer. Coarse aggregate is dense corundum, medium grain aggregate is plate corundum, fine aggregate is electrofused white corundum, added aluminum-rich spinel mass and electrofused magnesia sand, ultrafine aggregate is αAl2O3 and SiO2, the concluding agent is CA-80 steel, and the tonic is a water reducer. The mass ratio of antioxidant bone powder is about 37

If you are interested refractory products, contact us now!
Email: info@zaferroalloy.com Whatsapp: 8615896822096