One Of High Level Materials Silicon Briquette
Products Description
A method for spheroidizing low-silicon briquette agents for the production of ductile iron is characterized by using a square steel pipe to internally layer powdered materials containing a magnesium-silicon alloy with a silicon content of 10-20% and a magnesium content of 12-15%, with a total silicon content of 15-25%, calcium content of 1-2%, rare earth elements (RE) content of 0.5-1%, and the remainder being iron, along with a rare earth silicon iron alloy containing ≤5% magnesium, to form an integrated spheroidizing agent. A rectangular metal magnesium block is placed within the open-ended outer square steel pipe, and the space between the rectangular metal magnesium block and the outer square steel pipe is insulated with a compact refractory material, resulting in a spheroidizing agent made up of the outer square steel pipe and the compact refractory material surrounding the rectangular metal magnesium block. The above spheroidizing agent is placed in a spheroidizing vessel built with a reaction chamber and compacted within the square steel pipe using a press, followed by spheroidizing treatment using the pouring technique.
Products parameters
| Type | Si | C | S | P | Al |
| Si50# | 50 | 8 0.1 0.05 5 | |||
| Si50# | 50 | 15 | 0.1 | 0.1 | 3 |
| Si55# | 55 | 7 | 0.1 | 0.05 | 5 |
| Si60# | 60 | 5 | 0.08 | 0.05 | 5 |
| Si65# | 65 | 5 | 0.08 | 0.05 | 5 |
Products cooperation picture

1.A preparation method for nanometer mesoporous silicon briquette, characterized by the following process steps: at room temperature, slowly add sodium silicate solution containing 1%-10% silica into a strong inorganic acid of equivalent concentration 0.3-2N, stirring for 0.5-1 hour, until the pH of the reaction mixture is 2-3. The resulting acidic silica sol is then treated with strong acidic cation resin and weak basic anion resin to remove Na+ and inorganic acid anions, yielding acidic active silica sol. Mix 3-10 parts of the acidic active silica sol with 1-6 parts of water-soluble organic solvent, stir, and then mix with 3-9 parts of a template agent, stirring for 0.5-1 hour. Mix 10-18 parts of ammonia solution with a concentration of 5-15% with 2-8 parts of water-soluble organic solvent, stir for 0.5-1 hour, then mix with 1-6 parts of template agent, stirring for another 0.5-1 hour. Slowly add the resulting mixture (c) into the mixture obtained from step (b), stir for 0.5-1 hour, raise the temperature to t=25-50℃, and maintain a constant temperature for 0.5-1 hour; then raise the temperature to t=50-100℃, let it stand for 30-50 hours, filter, wash with distilled water 3-5 times, and finally calcine at 450-550℃ to produce mesoporous silica spheres.
Hot Tags: one of high level materials silicon briquette, China one of high level materials silicon briquette manufacturers, suppliers, factory